I-Metal foam ineempawu ze-porosity ephezulu, indawo enkulu yendawo ethile, i-ductility efanelekileyo kunye ne-thermal conductivity ephezulu, kwaye ineempawu ezilungileyo ze-hydrodynamic. Ineengenelo ezibaluleke kakhulu kwiintshukumo zegesi kunye nolwelo. Kwi-catalytic reaction, i-nickel-based-foam-based okanye i-copper-based metal ingasetyenziswa ngokuthe ngqo njenge-catalyst, okanye isinyithi esinegwebu sinokusetyenziswa njenge-catalyst carrier, kunye nezinye izinto ezinokuthi zifakwe kwi-surface layer. Isetyenziswa kwiindlela ezintathu ze-catalysis yokuphuma kwemoto, ukusabela kweekhemikhali zonyango, njl.
Iinkcukacha zeMveliso:
| Uhlobo | Vula iseli |
| Ubunyulu | > 99% |
| Ifom | Ishiti okanye Roll, kuxhomekeke kubukhulu & ubukhulu |
| Ubungakanani beSeli (PPI) | 10-150PPI, ngokwesicelo ngasinye |
| Ukutyeba | Umgangatho: 1-30mm Owongezelelweyo obhityileyo (30mm) unokwenziwa ngokwesicelo |
| Ubungakanani kunye noBume | Umgangatho: 500 * 500mm / 200 * 300mm; ingenziwa ngokwemilo eyahlukeneyo ngokwesicelo ngasinye |
| I-Porosity | 95%-98% |
| Vula izinga leSeli | ≥98 % |
| Ukuxinana koMqulu | >0.1g/cm3, ngokwesicelo ngasinye |
| Ukuxinana komphezulu | 200-2500 g/m ^2, ngokwesicelo ngasinye |
| I-Thermal Conductivity (Ithiyori) | >3W/MK |
| Amandla oomatshini (Ithiyori) | ≥2~7MPa |
| Amandla Okuqina (Ithiyori) | 8 ~ 50MPa |
| Ukumelana noBuqondo (Ithiyori) | ≥500℃ |
| Ubunzima beMolekyuli | 58.68 |
| Indawo yokunyibilika | 1455 °C |
| Indawo yokubilisa | 2732 °C |
| Ubushushu obuthile | 0.44 kJ/kg·K |
| Vickers Ukuqina | 638 MPa |
| Ukuxinana kweAreal | 350±20g/m2 |
| Ukuhanjiswa kombane | 69.3 nΩ·m (20 °C) |
Ixesha lokuposa: Sep-23-2022